In general even though energy is lost during hysteresis it is not called as heat losses . Generally I2R losses are called as heat losses because in these tye of only in these energy is lost in the form of real heat
what is hysteresis losses
Hysteresis losses depend on the type of metal used to manufacture the magnetic circuit of a machine. Most magnetic circuits are made from silicon steel. Generally speaking, there's not much you can do to reduce hysteresis losses as that has already been factored in by the machine's designer.
Hysteresis and eddy current loss constitute core loss. It can be reduced by replacing solid core by laminated core... by adeeb
Just like a transformer, the core losses are a combination of eddy current losses and hysteresis losses.
P/Vol=A/T P: Power Vol: Volume A: Area T: Period
what is hysteresis losses
hysteresis loss = N1/N2 R2/R1 C1/A1 (area of the loop)(vertical sensitivity) (horizontal sensitiivity
No
This loss of heat is considered a physical change.
No, you're hysteresis losses are set by Bmax, frequency, and material. The function is highly nonlinear and the loss goes up disproportionately with Bmax. When designing power transformers, you typically want the hysteresis + eddy losses to equal the copper losses.
To minimize hysteresis loss
Hysteresis losses depend on the type of metal used to manufacture the magnetic circuit of a machine. Most magnetic circuits are made from silicon steel. Generally speaking, there's not much you can do to reduce hysteresis losses as that has already been factored in by the machine's designer.
Hysteresis losses are a function of the magnetic characteristics of the magnetic circuit, so there is very little you can do to minimise hysteresis losses other than to reduce the primary voltage to a transformer if that is at all practicable. These losses are really in the hands of the manufacturers who design and manufacture magnetic circuits.
produces magnetic properties,such as small hysteresis area and permeability Hysteresis loss depends upon the material of the core
hysteresis loss= K B^1.6 egs/sec where k is STEINMEITZ coefficient and B is the maximum magnetic flux density
to reduce the eddy current loss in the machine
soft iron B-H curve area is very high and hysteresis loss is proportional to it frequency or no of loop cycles per sec and area of loop so hysteresis loss increases in soft iron as electro magnet