The chemical composition of 420 grade stainless steel is:- Chromium: 12-14 %-Silicon: max. 1 %- Manganese: max 1 %- Phosphorus: max. 0,04 %- Sulfur: max. 0,03 %- Carbon: min. 0,015 %
7.85kg per sq meter
7850 kg/m^3
16 m m steel rod weight per meter = 1.5816 m m steel rod of 12metres weights = 12 * 1.58 = 18.96 kg
formula calculation of steel round bar > Area (square metres) of cross section * 7850 = kilograms per metre length. For other lengths, multiply answer by length in metres.
What is the weight of 50x50x5 mm mild steel angle per metre length? Density mild steel is 7.85 g/cm3 Volume is 2x(4.5x0.5x100)+(0.5x0.5x100)=475 cm3 Weight is 7.85x475=3728.75 g (per metre).
Calculate the volume first by multiplying the cross sectional area with length.Multiply the volume with density of mild steel which will give the weight.The density of Mild steel is 7850 kg/ m3e.gCalculate the weight of 2 m rod having cross sectional area of 5 m2Volume = 2x5 = 10 m3Weight = 10 x 7850 = 78500 kgBe specific that same units are used all around the calculations.
The density of austenitic steel varies according to the type or grade. For one of the commonly used austenitic steel like Type 304, the density is 8.0g/cm3.
Sound velocity in steel - 5960 m/s Sound velocity in Stainless steel - 5760 m/s
Stainless steel 430 has the density rho = 7,750 kg/m3 or rho = 7.75 g/cm3.
7.184E-07 ohm-m
7390 m/s
As current passes through steel, it heats up from resistive heating. As it heats up, it expands. A typical coefficient of thermal expansion for steel is 13x10-6 m/m K but the exact coefficient of thermal expansion of steel depends on the type of steel. For example:Coefficient of Linear Thermal Expansion for:(10-6 m/m K)(10-6 in/in oF)Steel13.07.3Steel Stainless Austenitic (304)17.39.6Steel Stainless Austenitic (310)14.48.0Steel Stainless Austenitic (316)16.08.9Steel Stainless Ferritic (410)9.95.5
$990
7850 kg/m^3
Tin is a metal, so your question is nonsensical.
M. L. Glenn has written: 'Low-chromium heat-resisting ferritic alloys strengthened by the chi phase' -- subject(s): Chromium-iron alloys, Heat resistant alloys, Intermetallic compounds, Precipitation hardening 'Reduced-chromium stainless steel substitutes containing silicon and aluminum' -- subject(s): Austenitic stainless steel, Silicon steel, Stainless Steel, Steel-aluminum alloys
73 N-m for Dry Type / 66N-m for Lubricated
C.S density is 7.85 kg/m^3 it is wrong. the correct density for c.s. is 7.85 kg/dm3 the CS density is normally given as 7.85gm/cm^3 or 7850 kg/m^3