answersLogoWhite

0


Best Answer

It will corrode (eat) holes in aluminum- or eat it all up.

User Avatar

Wiki User

8y ago
This answer is:
User Avatar
More answers
User Avatar

AnswerBot

1w ago

Anodized aluminum is generally resistant to hydrochloric acid due to the hard oxide layer created during the anodization process. However, prolonged exposure to concentrated hydrochloric acid may still damage the anodized layer and affect the aluminum underneath.

This answer is:
User Avatar

User Avatar

Wiki User

14y ago

Yes, Formula:

Al203+6HCl -> 2AlCl3+3H20

-Kill_Me0215

This answer is:
User Avatar

User Avatar

Wiki User

11y ago

no

This answer is:
User Avatar

Add your answer:

Earn +20 pts
Q: Is anodized aluminum resistant to hydrochloric acid?
Write your answer...
Submit
Still have questions?
magnify glass
imp
Related questions

What happen when you put aluminum foil on hydrochloric acid?

if you put aluminum foil on hydrochloric acid it can flow joke! hehe


What happens when you put hydrochloric acid on Aluminum?

Hydrochloric acid reacts with aluminum to produce aluminum chloride and hydrogen gas. The reaction is exothermic and can cause the acid to fizz and release gas. In addition, the aluminum may corrode or dissolve in the acid.


What happens when aluminum and hydrochloric acid are mixed?

When aluminum and hydrochloric acid are mixed, a chemical reaction occurs where aluminum chloride and hydrogen gas are produced. The reaction is exothermic, meaning it releases heat, and can be quite vigorous depending on the concentration of the acid. It is important to handle this reaction with caution as it can produce flammable hydrogen gas.


Will sulfuric acid or hydrochloric acid corrode aluminum?

Yes, both sulfuric acid and hydrochloric acid can corrode aluminum. However, hydrochloric acid is generally considered less aggressive towards aluminum compared to sulfuric acid. The rate of corrosion depends on factors such as concentration, temperature, and exposure time.


Which acid or alkali will dissolve aluminum but not nickel?

Hydrochloric acid can dissolve aluminum but not nickel. Aluminum forms a soluble aluminum chloride compound in hydrochloric acid, while nickel does not react with hydrochloric acid due to its passivation layer.


Is mixing aluminum and hydrochloric acid a chemical change?

Be careful with your terminology.Mixing aluminum and hydrochloric acid is not a chemical change.The resulting reaction, however, is a chemical change.


What happens when hydrochloric acid is mixed with liver?

When hydrochloric acid is mixed with liver, the acid denatures the proteins in the liver tissue. This breakdown of proteins can affect the structure and function of enzymes and other molecules in the liver. Additionally, the acid can also disrupt the cellular membranes in the liver cells, leading to cell damage or destruction.


What is the word equation for the chemical reaction between alluminium hydroxide and hydrochloric acid?

The word equation for the reaction between aluminum hydroxide (Al(OH)3) and hydrochloric acid (HCl) is aluminum hydroxide + hydrochloric acid → aluminum chloride + water.


Is aluminum more reactive with hydrochloric acid or sodium hydroxide?

aluminum will produce tiny bubbles


Balanced Equation for aluminum and hydrochloric acid?

2Al + 3Cl2 -> 2AlCl3


What isEquation for aluminum and hydrochloric acid?

2Al + 6HCl >> 2AlCl3 + 3H2


Will a single replacement reaction occur for aluminum and hydrochloric acid?

Yes, a single replacement reaction will occur between aluminum and hydrochloric acid. The aluminum will replace the hydrogen in the hydrochloric acid, forming aluminum chloride and hydrogen gas as products.