Delrin, a brand name for acetal (polyoxymethylene), does not have a hardness value on the Mohs scale, as this scale is typically used for minerals. However, Delrin has a Shore D hardness of approximately 80 to 90, indicating it is a relatively hard plastic. This hardness makes it suitable for various applications requiring durability and resistance to wear.
diamond
Muscovite mica has a hardness of around 2-2.5 on the Mohs scale.
Yes "feldspar" is one of the minerals on Moh's scale of hardness.
Friedrich Moh
it is a geological scale that measures the hardness of different minerals. Talc being the softest and a diamond being the hardest.
The hardness of conundrum is 9 on the Moh's hardness scale
Hardness is 7.5 to 8
About 5 on Moh's hardness scale.
It depends on the deposit. What deposit are you talking about? What measure of hardness are you after? e.g. UCS, Moh's Hardness Scale e.t.c. On moh it is 4 Brinnel hardness it is 490
moh's hardness scale and??
The Moh's hardness of Barium Sulfate is 3. It is very low in abrasion.
Hardness of a mineral - the answer in in the title "Moh's hardness scale".
The hardness of lead is about 2.5 on moh's hardness scale. hope this helped wanka
Halite, with a hardness of 2.5 on the Moh's Scale, is very soft.
What is Mohs hardness of Barium Sulfate
Diamond
Talc.