AA6360 is an alloy coming under AA6xxx series, the elements predominant in AA6360 are Magnesium and silicon with added traces of Mn, Cu, Cr, Zn, Ni and Ti. It is generally in the heat treated condition i.e., it can be solution heat treated and artificially aged. Its minimum ultimate tensile strength and minimum yield strength are 206.843 MPa and 172.3689 MPa respectively.